Alternate Names: Potassium chloride, KCL, Silvin, Silvine
Description: Soluble source of K2O
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 52.44% | 1.00 | |
| Cl | 47.56% | n/a | |
| Oxide Weight | 94.20 | ||
| Formula Weight | 179.63 | ||
This can be used as an alternative to NaCl in the salt glaze process.
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Oxides | K2O - Potassium Oxide |
| Minerals |
Sylvite
Soluble source of K2O. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk