Description: Zirconium silicate

Oxide Analysis Formula Tolerance
ZrO2 67.21% 1.00
SiO2 32.79% 1.00
Oxide Weight 183.34
Formula Weight 183.34

Notes

Also known as Zircopax Plus or Ultrox (see link below for more information).

Related Information

Links

Materials Zircopax Plus
Materials Zircon
Zircon (zirconium silicate) is a hard, dense, refractory ceramic material used to opacify pottery glazes and in refractory products such as kiln washes, crucibl
Materials Ultrox