Description: Pinks/Crimsons (CrAl, CrAlZn)
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Stain
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Glaze Color | According to Mason Color: This type of pigment requires the correct glaze chemistry in all temperature ranges, in order to maximize the "color value". High calcium content is most important, and zinc & magnesia must be low to zero. Boron should not be too high. A major complication is that these rules do not necessarily apply when "fast-firing" techniques are used. Second, these pigments need an oxidizing atmosphere throughout the firing cycle. |
|---|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk