Spinks 105

Description: Deflocculant

Notes

A sodium polyacrylate dispersant used to deflocculate clay suspensions. Deflocculation results in a lowering of the viscosity of the clay suspension, which allows more solids (clay) to be introduced, thereby increasing the specific gravity and reducing the amount of water, absorbed by the plaster mold.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Electrolyte
Materials used to control slurry properties of glazes and slips (vicosity, specific gravity).

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy