SP-G Feldspar

Description: Sodium/potassium/calcium Feldspar

Oxide Analysis Formula Tolerance
CaO 1.40% 0.14
K2O 4.10% 0.24
Na2O 6.82% 0.62
Al2O3 18.92% 1.04
SiO2 68.15% 6.35
Fe2O3 0.06% -
LOI 0.08%n/a
Oxide Weight 557.21
Formula Weight 557.65

Notes

Used as an alumina source in glass batch formulations. Beneficiated using the froth flotation process for low iron oxide content.

Related Information

Links

Materials G-200 Feldspar
Materials NC-4 Feldspar
Materials Calcium Feldspar
Materials Potash Feldspar
A feldspar having a KNaO content that predominates in potassium.
Materials Soda Feldspar
A feldspar having a KNaO content that predominates in sodium.
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

Data

Bulk Density lbs/cu. ft. (Packed) 80

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy