Sodium Carbonate Decahydrate

Alternate Names: Washing Soda, Hydrous Sodium Carbonate

Formula: Na2CO3.10H2O

Oxide Analysis Formula Tolerance
Na2O 21.68% 1.00
CO2 15.38%n/a
H2O 62.94%n/a
Oxide Weight 62.00
Formula Weight 285.98

Related Information

Links

Materials Sodium Carbonate
Materials Sodium Carbonate Heptahydrate
Materials Sodium Bicarbonate
Hazards Sodium Carbonate Toxicology
Typecodes Electrolyte
Materials used to control slurry properties of glazes and slips (vicosity, specific gravity).

Data

Frit Softening Point 34C D
Density (Specific Gravity) 1.44

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy