| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 73.00% | 9.26 | |
| Al2O3 | 16.00% | 1.20 | |
| K2O | 7.40% | 0.60 | |
| Na2O | 2.60% | 0.32 | |
| CaO | 0.60% | 0.08 | |
| TiO2 | 0.20% | 0.02 | |
| Oxide Weight | 760.75 | ||
| Formula Weight | 760.75 | ||
| Materials |
Cornwall Stone
Cornwall stone was a low-iron feldspar material used primarily as a flux in clay bodies and glazes |
| URLs |
https://www.lagunaclay.com/_files/ugd/e5330f_7db9a3fbb7f34169a22ab4151512d40b.pdf
SG919 Cornwall Stone substitute from Laguna Clay Article at their website comparing this with Cornwall stone and MFW30/G Spray Dried Flux. |
| URLs |
https://www.lagunaclay.com/_files/ugd/e5330f_deb4b5cce2c7486c98fcfc499603bd73.pdf
SG919 Cornwall Substitute SDS |