RC10 Vitreous

Oxide Analysis Formula Tolerance
SiO2 71.40% 5.51
Al2O3 22.00% 1.00
Fe2O3 0.65% 0.02
TiO2 0.29% 0.02
Na2O 2.80% 0.21
K2O 1.30% 0.06
CaO 1.00% 0.08
MgO 0.20% 0.02
LOI 0.30%n/a
Oxide Weight 461.97
Formula Weight 463.36

Related Information

Links

Materials RC4 Vitreous
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Bulk Density g/cc (Packed) 1.4
Hardness (Moh) 7
Ultimate Particle Size Distribution >100 micron: 2%
Density (Specific Gravity) 2.6
pH for dry powder 7-8

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy