Description: High alkali frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 6.31% | 0.20 | |
| K2O | 15.90% | 0.30 | |
| SiO2 | 50.71% | 1.50 | |
| Na2O | 17.44% | 0.50 | |
| Al2O3 | 5.74% | 0.10 | |
| B2O3 | 3.91% | 0.10 | |
| Oxide Weight | 177.78 | ||
| Formula Weight | 177.78 | ||
Made by Podmore and Sons
Formerly Frit T
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Potclays Frit 2275
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |