Pemco Frit Pb-704

Alternate Names: Frit Pb704

Description: Zinc bearing, all-fritted base for cone 1-6

Oxide Analysis Formula Tolerance
BaO 2.60% 0.04
CaO 9.20% 0.39
K2O 3.50% 0.09
MgO 0.30% 0.02
Na2O 2.10% 0.08
PbO 6.60% 0.07
ZnO 10.60% 0.31
ZrO2 0.50% 0.01
B2O3 5.20% 0.18
Al2O3 5.10% 0.12
SiO2 54.30% 2.16
Oxide Weight 238.54
Formula Weight 238.54

Related Information

Links

Materials Pemco Frit Pb-197
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 2GF56C
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.70
Co-efficient of Linear Expansion 6.7 x 10-6 (40-450C)
Frit Softening Point 1500F
Frit Melting Range (C) 1450-1650F
I.F.P. (celsius) 683C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy