Pemco Frit Pb-700

Alternate Names: Frit Pb700

Description: Lead alumina bilsilicate frit (1% alumina)

Oxide Analysis Formula Tolerance
PbO 64.99% 1.00
Al2O3 1.01% 0.03
SiO2 34.00% 1.94
Oxide Weight 343.44
Formula Weight 343.44

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Hommel Frit 28
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.8 x 10-6 (40-450C)
Frit Melting Range (C) 1320-1450F
I.F.P. (celsius) 552C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy