Alternate Names: Frit Pb1951
Description: Lead-borosilicate flux
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 63.20% | 1.00 | |
| B2O3 | 19.70% | 1.00 | |
| SiO2 | 17.10% | 1.00 | |
| Oxide Weight | 353.16 | ||
| Formula Weight | 353.16 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.50 |
|---|---|
| Co-efficient of Linear Expansion | 8.5 x 10-6 (50-350C) |
| Frit Softening Point | 1000F |
| Frit Melting Range (C) | 960-1080F |
| I.F.P. (celsius) | 415C |