Pemco Frit P-4K05

Alternate Names: 4K05,4K-05

Description: Moderate melting Zirconia frit

Oxide Analysis Formula Tolerance
CaO 6.00% 0.48
K2O 2.80% 0.13
Na2O 4.60% 0.33
ZnO 1.10% 0.06
ZrO2 8.50% 0.31
B2O3 13.20% 0.85
Al2O3 7.60% 0.33
SiO2 56.20% 4.17
Oxide Weight 445.67
Formula Weight 445.67

Notes

Similar to Fusion Frit FZ-376A, chemistry shown here was copied, not exact.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit FZ-376A
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.54
Frit Softening Point 925C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy