Pemco Frit P-1F07

Alternate Names: 1F07,1F-07

Description: High CaO/Na2O/ZnO borosilicate low alumina frit

Oxide Analysis Formula Tolerance
BaO 3.70% 0.04
CaO 14.30% 0.44
K2O 1.10% 0.02
MgO 0.40% 0.02
Na2O 9.60% 0.27
ZnO 9.70% 0.21
Sb2O3 0.10% -
B2O3 20.20% 0.51
Al2O3 4.30% 0.07
SiO2 36.10% 1.05
Oxide Weight 173.15
Formula Weight 173.15

Notes

For partially-fritted textured glazes.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.30
Co-efficient of Linear Expansion 9.30 (50-450C)
Frit Softening Point 1450F
Frit Melting Range (C) 1380-1540F
Co-efficient of Linear Expansion 9.5x10-6 (50-450C)
I.F.P. (celsius) 690C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy