Alternate Names: 1A44,1A-44
Description: Low expansion high zinc high boron frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZnO | 59.50% | 1.00 | |
| B2O3 | 32.50% | 0.64 | |
| SiO2 | 8.00% | 0.18 | |
| Oxide Weight | 136.81 | ||
| Formula Weight | 136.81 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Pemco Frit P-1A43
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 4.60 |
|---|---|
| Co-efficient of Linear Expansion | 4.60 (50-450C) |
| Frit Softening Point | 1400F |
| Frit Melting Range (C) | 1350-1450F |
| I.F.P. (celsius) | 660C |