Alternate Names: Frit 1836, Frit P1836
Description: Leadless, high zinc, all-fritted glaze
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 6.70% | 0.11 | |
| CaO | 7.10% | 0.32 | |
| K2O | 1.10% | 0.03 | |
| Na2O | 3.80% | 0.16 | |
| ZnO | 12.30% | 0.38 | |
| B2O3 | 3.10% | 0.11 | |
| Al2O3 | 7.10% | 0.18 | |
| SiO2 | 58.80% | 2.48 | |
| Oxide Weight | 253.59 | ||
| Formula Weight | 253.59 | ||
Used on regular and fast-fire wollastonite and talc bodies.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.1 x 10-6 (50-450C) |
|---|---|
| Frit Melting Range (C) | 1500-1700F |