| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 1.20% | 0.07 | |
| MgO | 10.30% | 0.87 | |
| K2O | 1.20% | 0.04 | |
| Na2O | 0.20% | 0.01 | |
| Al2O3 | 13.20% | 0.44 | |
| SiO2 | 69.50% | 3.95 | |
| Fe2O3 | 4.50% | 0.10 | |
| Oxide Weight | 341.71 | ||
| Formula Weight | 341.71 | ||
The same as attapulgite, this is just another sample analysis.
| Materials |
Attapulgite
|
| Materials |
Sepiolite
|
| Typecodes |
Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate. |
| Minerals |
Attapulgite, Palygorskite
Attapulgite is a magnesium aluminum silicate clay of very fine particle size. It is also known as Fu |