P8 Quartz

Oxide Analysis Formula Tolerance
CaO 0.04% 0.15
K2O 0.10% 0.22
TiO2 0.03% 0.08
Al2O3 0.50% 1.00
SiO2 99.10% 336.38
Fe2O3 0.04% 0.05
LOI 0.20%n/a
Oxide Weight 20,361.24
Formula Weight 20,402.04

Related Information

Links

Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO
Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.

Data

Bulk Density g/cc (Packed) 1.2
Hardness (Moh) 7
Ultimate Particle Size Distribution >45 micron: 1.4%
Density (Specific Gravity) 2.6
pH for dry powder 8-9

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy