Ohio #3 Fireclay

Oxide Analysis Formula Tolerance
Al2O3 27.69% 1.00
SiO2 55.75% 3.42
K2O 2.96% 0.12
TiO2 1.99% 0.09
Fe2O3 2.28% 0.05
MgO 1.15% 0.11
LOI 8.17%n/a
Oxide Weight 338.23
Formula Weight 368.32

Related Information

Links

Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy