No 2 Missouri Flint Clay

Oxide Analysis Formula Tolerance
SiO2 51.20% 2.74 .3
Al2O3 31.70% 1.00 .5
Fe2O3 1.40% 0.03 .3
TiO2 2.00% 0.08 .1
K2O 1.10% 0.04 .4
MgO 0.35% 0.03 .05
CaO 0.80% 0.05 .4
P2O5 0.70% 0.02 .3
Na2O 0.10% 0.01
LOI 13.30%n/a
Oxide Weight 287.50
Formula Weight 331.60

Notes

A semi-plastic Missouri Flint clay. It is well suited for brick and tile manufacturers.

Related Information

Links

Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy