Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability recently discovered. Servers were upgraded ahead of schedule on Oct 21. This could cause some issues. Please contact us if you encounter any.
Alternate Names: NiO, Nickelous oxide, Green Nickel Oxide, Nickel(II) oxide
Formula: NiO
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| NiO | 100.00% | 1.00 | |
| Oxide Weight | 74.70 | ||
| Formula Weight | 74.70 | ||
| Materials |
Nickel Carbonate
|
| Materials |
Nickel Oxide Black
|
| Hazards |
Nickel Compounds Toxicity
|
| Typecodes |
Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials. |
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| URLs |
http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc09/icsc0926.htm
Nickel Oxide Hazards at ilo.org |
| URLs |
https://en.wikipedia.org/wiki/Nickel(II)_oxide
Green Nickel Oxide at Wikipedia |
| Oxides | NiO - Nickel Oxide |
| Frit Softening Point | 1984C |
|---|---|
| Density (Specific Gravity) | 6.6- 7.5 |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk