Moulin Fritte M1511

Alternate Names: Fritte M 1511

Description: Fritte Boro-acaline Plombeuse

Oxide Analysis Formula Tolerance
PbO 36.90% 0.50
B2O3 23.10% 1.01
Na2O 10.20% 0.50
SiO2 29.80% 1.50
Oxide Weight 303.18
Formula Weight 303.18

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 504C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy