Description: Calcium alkaline leadless high borax frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 6.27% | 0.14 | |
| CaO | 14.94% | 0.54 | |
| ZnO | 3.10% | 0.08 | |
| MgO | 0.57% | 0.03 | |
| Na2O | 6.49% | 0.21 | |
| Al2O3 | 13.58% | 0.27 | |
| B2O3 | 26.48% | 0.78 | |
| SiO2 | 28.58% | 0.97 | |
| Oxide Weight | 204.20 | ||
| Formula Weight | 204.20 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |