| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.66% | 0.67 | |
| K2O | 0.54% | 0.02 | |
| Na2O | 5.54% | 0.31 | |
| B2O3 | 13.23% | 0.67 | |
| Al2O3 | 13.51% | 0.46 | |
| SiO2 | 56.51% | 3.30 | |
| Oxide Weight | 350.71 | ||
| Formula Weight | 350.71 | ||
Calculated raw sub:
Gerstely Borate 19.5
Pioneer Kaolin 15.0
Flint 25.0
Whiting 8.5
Nepheline Syenite 19
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk