Description: High boron zero silicate calcia alumina frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| B2O3 | 70.00% | 4.27 | |
| Al2O3 | 24.00% | 1.00 | |
| CaO | 4.00% | 0.30 | |
| Oxide Weight | 416.50 | ||
| Formula Weight | 416.50 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |