Alternate Names: M 136,M-136
Description: Natriubor-Silikat
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 0.45% | 0.17 | |
| CaO | 0.45% | 0.69 | |
| K2O | 0.15% | 0.14 | |
| B2O3 | 0.45% | 0.56 | |
| Al2O3 | 0.15% | 0.13 | |
| SiO2 | 1.75% | 2.50 | |
| Oxide Weight | 292.35 | ||
| Formula Weight | 292.35 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 67 |
|---|---|
| Frit Softening Point | 603C |