Description: Alkali-Zink-Boor Fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 5.05% | 0.28 | |
| Li2O | 0.86% | 0.09 | |
| Al2O3 | 11.48% | 0.35 | |
| SiO2 | 61.09% | 3.16 | |
| K2O | 10.60% | 0.35 | |
| ZnO | 7.33% | 0.28 | |
| B2O3 | 3.58% | 0.16 | |
| Oxide Weight | 311.06 | ||
| Formula Weight | 311.06 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |