Description: Alkali Fritte
Oxide | Analysis | Formula | |
---|---|---|---|
Al2O3 | 3.06% | 0.06 | |
SiO2 | 63.12% | 2.10 | |
CaO | 2.81% | 0.10 | |
K2O | 2.83% | 0.06 | |
Na2O | 19.23% | 0.62 | |
ZnO | 8.96% | 0.22 | |
Oxide Weight | 199.87 | ||
Formula Weight | 199.87 |
Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
---|---|
Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |