| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 41.70% | 0.54 | |
| P2O5 | 54.00% | 0.46 | |
| B2O3 | 4.30% | 0.08 | |
| Oxide Weight | 121.47 | ||
| Formula Weight | 121.47 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 681C |
|---|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |