| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 45.70% | 0.77 | |
| P2O5 | 20.40% | 0.23 | |
| B2O3 | 33.90% | 0.77 | |
| Oxide Weight | 159.01 | ||
| Formula Weight | 159.01 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 770C |
|---|