Johnson Matthey Frit 169

Alternate Names: Frit NR169, Fritte NR 169, Frit NR 169

Description: Barium frit

Oxide Analysis Formula Tolerance
Na2O 19.20% 0.64
CaO 2.30% 0.09
BaO 9.10% 0.12
ZnO 5.80% 0.15
B2O3 28.40% 0.85
Al2O3 0.30% 0.01
SiO2 34.90% 1.21
Oxide Weight 207.78
Formula Weight 207.78

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Johnson Matthey Frit 623
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 700 C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy