Description: OPAQUE (FORMERLY #90401050)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 14.00% | 0.69 | |
| KNaO | 4.00% | 0.14 | |
| ZnO | 9.00% | 0.31 | |
| ZrO2 | 9.00% | 0.20 | |
| B2O3 | 7.00% | 0.28 | |
| Al2O3 | 6.00% | 0.16 | |
| SiO2 | 50.00% | 2.31 | |
| Oxide Weight | 274.91 | ||
| Formula Weight | 274.91 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 0.293 @ 500C |
|---|