Description: Opaque (formerly #90401026)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 6.00% | 0.74 | |
| KNaO | 8.00% | 0.71 | |
| ZnO | 3.00% | 0.26 | |
| ZrO2 | 8.00% | 0.45 | |
| B2O3 | 12.00% | 1.20 | |
| Al2O3 | 9.00% | 0.61 | |
| SiO2 | 54.00% | 6.25 | |
| Oxide Weight | 695.38 | ||
| Formula Weight | 695.38 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 0.316 @ 500C |
|---|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk