Description: TRANSPARENT (FORMERLY #FT0541)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 1.00% | 0.03 | |
| CaO | 8.00% | 0.64 | |
| KNaO | 7.00% | 0.40 | |
| ZnO | 6.00% | 0.33 | |
| B2O3 | 8.00% | 0.52 | |
| Al2O3 | 10.00% | 0.44 | |
| SiO2 | 58.00% | 4.33 | |
| Oxide Weight | 439.79 | ||
| Formula Weight | 439.79 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 0.308 @ 500C |
|---|