| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.02% | - | |
| K2O | 3.20% | 0.14 | |
| MgO | 0.47% | 0.05 | |
| Al2O3 | 25.20% | 1.00 | |
| SiO2 | 61.20% | 4.12 | |
| Fe2O3 | 1.74% | 0.04 | |
| TiO2 | 1.04% | 0.05 | |
| Na2O | 0.16% | 0.01 | |
| LOI | 11.00% | n/a | |
| Oxide Weight | 376.55 | ||
| Formula Weight | 423.09 | ||
Manufacturer says: A nice white clay in the raw state. Fires to a cream color.
Physical data can be found on the link to the product information web page of the manufacturer.
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| URLs |
https://www.clayimco.com/industrial-clays
IMCO information on their mined clays |