Description: Zircon borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 6.03% | 0.49 | |
| Na2O | 6.06% | 0.45 | |
| ZnO | 1.00% | 0.06 | |
| ZrO2 | 12.38% | 0.46 | |
| B2O3 | 13.63% | 0.90 | |
| Al2O3 | 4.16% | 0.19 | |
| SiO2 | 56.72% | 4.34 | |
| Oxide Weight | 459.65 | ||
| Formula Weight | 459.65 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3302-D
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.00 |
|---|---|
| Frit Softening Point | 1720F |