Hommel Frit 486

Description: Calcium strontium borosilicate frit

Oxide Analysis Formula Tolerance
K2O 2.17% 0.07
Na2O 3.40% 0.16
CaO 10.43% 0.54
MgO 0.51% 0.04
BaO 0.13% -
PbO 4.24% 0.06
SrO 3.81% 0.11
Li2O 0.36% 0.04
Al2O3 7.06% 0.20
B2O3 8.98% 0.37
SiO2 58.80% 2.83
Oxide Weight 289.41
Formula Weight 289.41

Related Information

Links

Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.6 x 10-6
Frit Softening Point 1600F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy