Description: Sodium borate zirconium frit (1% lead)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.65% | 0.04 | |
| Na2O | 7.23% | 0.72 | |
| CaO | 1.71% | 0.19 | |
| MgO | 0.09% | 0.01 | |
| PbO | 1.06% | 0.03 | |
| Al2O3 | 6.72% | 0.41 | |
| B2O3 | 15.87% | 1.42 | |
| SiO2 | 55.69% | 5.76 | |
| ZrO2 | 10.93% | 0.55 | |
| Oxide Weight | 620.90 | ||
| Formula Weight | 620.90 | ||
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.5 x 10-6 |
|---|---|
| Frit Softening Point | 1580F |