Description: LEADED
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 5.25% | 0.34 | |
| K2O | 2.03% | 0.08 | |
| Na2O | 1.76% | 0.10 | |
| PbO | 29.83% | 0.48 | |
| ZrO2 | 1.18% | 0.03 | |
| B2O3 | 11.93% | 0.62 | |
| Al2O3 | 3.12% | 0.11 | |
| SiO2 | 41.37% | 2.48 | |
| F | 3.53% | 0.67 | |
| Oxide Weight | 360.79 | ||
| Formula Weight | 360.79 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |