| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 6.36% | 0.35 | |
| CaO | 3.04% | 0.19 | |
| PbO | 29.94% | 0.46 | |
| B2O3 | 6.24% | 0.31 | |
| SiO2 | 44.32% | 2.53 | |
| TiO2 | 8.86% | 0.38 | |
| F | 1.24% | 0.22 | |
| Oxide Weight | 343.75 | ||
| Formula Weight | 343.75 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3482
|
| Materials |
Pemco Frit Pb-1151
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 9.2 x 10-6 (50-450C) |
|---|---|
| Frit Softening Point | 1650F |