Description: High Lead Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 8.21% | 0.30 | |
| PbO | 68.94% | 0.70 | |
| B2O3 | 11.98% | 0.39 | |
| SiO2 | 10.87% | 0.41 | |
| Oxide Weight | 226.61 | ||
| Formula Weight | 226.61 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |