Description: Synthetic version of UK Cornwall stone

Oxide Analysis Formula Tolerance
SiO2 77.39% 12.48
TiO2 0.05% 0.01
Al2O3 14.06% 1.34
Fe2O3 0.20% 0.01
CaO 0.42% 0.07
MgO 0.05% 0.01
Na2O 3.56% 0.56
K2O 3.34% 0.34
P2O5 0.22% 0.02
Oxide Weight 962.55
Formula Weight 962.55

Notes

Formulated as a substitute for UK Cornwall Stone for use in North America.

This was described in an article in Ceramics Technical Nov 2011. The chemistry has some significant differences to the standard UK Cornwall Stone (e.g. 5% more SiO2, 0.4% CaO vs. 1.8%, 6.9% KNaO vs. 7.6%). These suggest that it will not melt as quite as well, testing should be done.

Related Information

Links

Materials Cornwall Stone

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy