Description: High lead boron frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 0.30% | 0.02 | |
| PbO | 42.40% | 0.98 | |
| Al2O3 | 5.80% | 0.29 | |
| B2O3 | 10.20% | 0.75 | |
| SiO2 | 41.40% | 3.54 | |
| Oxide Weight | 513.85 | ||
| Formula Weight | 513.85 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |