Alternate Names: Fusion Frit F561
Description: Barium-Zircon Matte frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 5.00% | 0.23 | |
| B2O3 | 11.50% | 0.76 | |
| K2O | 5.30% | 0.26 | |
| BaO | 24.60% | 0.74 | |
| SiO2 | 46.00% | 3.53 | |
| ZrO2 | 7.60% | 0.28 | |
| Oxide Weight | 461.40 | ||
| Formula Weight | 461.40 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.5 x 10-6 |
|---|---|
| Frit Softening Point | 1800F |