Alternate Names: Fusion Frit F326
Description: Opaque frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 2.30% | 0.10 | |
| Na2O | 6.00% | 0.41 | |
| CaO | 4.50% | 0.34 | |
| MgO | 1.50% | 0.16 | |
| Al2O3 | 8.60% | 0.35 | |
| B2O3 | 10.60% | 0.64 | |
| SiO2 | 56.50% | 3.94 | |
| ZrO2 | 10.00% | 0.34 | |
| Oxide Weight | 419.07 | ||
| Formula Weight | 419.07 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.6 x 10-6 |
|---|---|
| Frit Softening Point | 1600F |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |