Description: Reimbold & Strick calcium matte frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| B2O3 | 10.00% | 0.25 | |
| CaO | 30.00% | 0.92 | |
| SiO2 | 54.00% | 1.54 | |
| Na2O | 3.00% | 0.08 | |
| Al2O3 | 3.00% | 0.05 | |
| Oxide Weight | 171.48 | ||
| Formula Weight | 171.48 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 80 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | >800C |
| Glass Transition Temperature | 602C |