Description: Reimbold & Strick stoneware frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 6.00% | 0.40 | |
| SiO2 | 61.00% | 4.22 | |
| B2O3 | 14.00% | 0.84 | |
| K2O | 2.00% | 0.09 | |
| MgO | 1.00% | 0.10 | |
| CaO | 3.00% | 0.22 | |
| BaO | 3.00% | 0.08 | |
| ZnO | 2.00% | 0.10 | |
| Al2O3 | 8.00% | 0.33 | |
| Oxide Weight | 415.91 | ||
| Formula Weight | 415.91 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 54 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | 640C |
| Glass Transition Temperature | 570C |