Alternate Names: Frit A3021
Description: Reimbold & Strick low expansion Ca-B frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.00% | 1.00 | |
| ZrO2 | 3.00% | 0.14 | |
| Al2O3 | 10.00% | 0.55 | |
| SiO2 | 51.00% | 4.76 | |
| B2O3 | 26.00% | 2.10 | |
| Oxide Weight | 561.00 | ||
| Formula Weight | 561.00 | ||

This picture has its own page with more detail, click here to see it.
I was impressed with this frit company, Reimbold & Strick. Their frit data was educational, by studying the chemistry of their matte frits, for example, you could see the various mechanisms that produce the effect. But, it is no longer available. However, with a little determination you could likely find the pages at the internet archive (see link below).
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 42 X 10-7 (20-400C) |
|---|---|
| Frit Softening Point | 710C |
| Glass Transition Temperature | 650C |