Frit A 2010

Description: Low melting lead borosilicate

Oxide Analysis Formula Tolerance
Na2O 6.00% 0.24
SiO2 13.00% 0.53
B2O3 12.00% 0.42
PbO 69.00% 0.76
Oxide Weight 246.36
Formula Weight 246.36

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Frit G-23
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 111 x 10-7 (20-400C)
Frit Softening Point 410C
Glass Transition Temperature 380C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy