Alternate Names: Frit VO6004p
Description: Israel
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 15.50% | 0.47 | |
| Na2O | 11.50% | 0.53 | |
| B2O3 | 25.50% | 1.05 | |
| Al2O3 | 3.50% | 0.10 | |
| SiO2 | 44.00% | 2.09 | |
| Oxide Weight | 285.69 | ||
| Formula Weight | 285.69 | ||
| Materials |
Degussa Frit 90198
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk